ANSERGLOB BCX

Advantages

  • High adhesion
  • Freezeproof
  • Ecologically friendly
  • Waterproof
  • Suitable for swimming pools
  • Suitable for natural stone

Technical data

Thickness of the layer 2-10 mm
Mixture ratio 0,21-0,22 L per kg of mixture
Deflection not less than 2,5 mm
Pot life not less than 2 hours
Open time not less than 20 min
Adjustment time not less than 15 min
Grouting 24 hours
Adhesion to substrate more than 1,5 MPa
Frost resistance not less than 50 cycles
Slip not more than 0,1 mm
Surface temperature from +5°С to +30°С
Operating temperature from -30°С to +80°С

Adhesive ANSERGLOB BCX 44 flexible is intended for interior and exterior facing surfaces subjected to periodic deformations (atmospheric influences and dynamic loads) with all types of tiles made of natural, artificial, and cast stone (except marble), as well as concrete, ceramic, and opaque glass tiles with dimensions not exceeding 1.0 x 1.0 m. The adhesive can be used for facing of swimming pools and tanks, monolithic floors, accessible roofs, terraces, concrete, brick, stone, asbestos-cement, and other strong surfaces. It can be applied for use with water and electric underfloor heating systems. The adhesive can be used for fixing thermal insulation boards made of polystyrene foam, polyurethane, mineral wool, and foam glass. The adhesive is effective for facing surfaces without removing old tiles ("tile-on-tile" method).


The surface preparation is realized according to State Standard of Ukraine (DSTU N B A.3.1-23:2013) and State Building Codes of Ukraine (DBN В.2.6-162:2010 and DBN В.2.6-22-2001). Surface must be structurally sound, clean, dry and free from dust, grease, dirt, lime, wax, oil or emulsion paints. Fragile areas of substrate must be removed. Surface irregularity till 10 mm must be leveled by adhesive mortar ANSERGLOB BCX 44, big irregularities of walls – by the plaster mortar ANSERGLOB ВСТ 20, big irregularities of floors of by cement screed ANSERGLOB LFS 69 or ANSERGLOB LFS 70. Before applying substrates with strong sorption must be treated by one of deeply penetrating emulsions ANSERGLOB and exposed for 4 hours. Before applying substrates with low sorption and also surfaces which are tiled by method “tile on tile” must be treated by ANSERGLOB EG 62 or ANSERGLOB EG 63 BETON KONTAKT and exposed from 3 to 6 hours.
Prepared mortar should be spread by tile trowel, spatula or float on cladding surface. After applied mortar is combed by notch trowel or spatula with the U-shaped notches or square notches, which form equal combs of the same altitude on applied surface. Depending on thickness and dimensions of cladding tiles notch size of trowel is selected (for example, for tile size 20x20 cm trowels with the square notch size 6 mm and more are used). Tiles are installed in turn on the surface, covered by adhesive mortar, and pressed evenly. The tile can be moved during 15 min from the moment of installation if required. Thickness of adhesive layer between tile and substrate must be minimally 2 mm to show its full curing. Using handmade tile with unleveled back side and some cut ceramic and stone tile additional spreading of adhesive mortar by rectangular trowel on tile back side is required in order to achieve full contact between tile and substrate. Applying of adhesive mortar on back side of tile is additional measure and does not replace its spreading on the substrate. Joint width between tiles must be not less than 1,5 mm.
Tiles are prohibited to wet preliminary!

Note: Application should be complied at temperature above +5°С and below +30°С. All the mentioned recommendations are effective at temperature of +20°С and air humidity of 60%. Under the other conditions crusting, stiffening and curing time may be changed.

Average consumption of the mixture is 1,3 kg per m2 on 1 mm of layer.
Dry mixture must be poured into container with clear water according to ratio 0,21-0,22 liters of water per 1 kg of mixture (5,25-5,5 liters of water per 1 bag of 25 kg) when at the same time manually or mechanically mixed (by the drill on low revs) to obtain the kindred and elastic mass. After exposing 5 min mortar must be mixed again and used during 2 hours.

Can be used with other our products

Related products

X

Become a reseller

Leave your contact information, we will contact you shortly to discuss cooperation

X

FORM FOAM

X

Thank you, the application has been successfully sent!
Our manager will contact you as soon as possible

X

Thanks, your order has been successfully sent!
Our manager will contact you shortly

X

I want to work in anserglob






(doc, docx, pdf)

Attach resume